Cooling patches, acupoint pressure patches, medical adhesive dressings and similar skin-applied devices often carry a line in their Chinese product technical requirements that reads "adhesion: tested according to Chinese Pharmacopoeia General Chapter 0952". The trouble is that Chapter 0952 contains four methods and leaves the incline angle, the steel ball number and the acceptance limit to "the individual monograph". A device has no monograph, so if the requirement only cites the chapter number, the laboratory cannot tell which method to run or how to judge the result. This article explains how the chapter is organised, walks through the two methods accredited at SUNGO's Shanghai laboratory (Method 1, initial tack; Method 3, peel strength), and covers how to write the requirement, how the chapter differs from YY/T 1627-2018, and what to prepare before testing.
Key points
- General Chapter 0952 (黏附力测定法, adhesion test method) is a general test method in Volume IV of the Chinese Pharmacopoeia (ChP); the 2025 Edition has been in force since 1 October 2025. It assesses the adhesion of medicated plasters and patches with four indicators: Method 1, initial tack; Method 2, holding power; Method 3, peel strength; Method 4, adhesive force.
- The chapter leaves the incline angle, the ball number to be held and the peel strength limit to the monograph. A device that borrows Chapter 0952 must state them in its product technical requirements; otherwise there is no basis for a pass or fail statement.
- The CNAS scope (L22083) and the CMA scope (240015340087) of Shanghai SUNGO Medical Technology Co., Ltd. both list "adhesion" to ChP 2025 Edition General Chapter 0952, with the test object "medical devices" and the limitation "Methods 1 and 3 only". The IAS scope does not include this item, and the Hefei laboratory is not involved.
- Method 2 (holding power) and Method 4 (adhesive force) are outside SUNGO's accredited scope and must be commissioned from another body with the relevant capability.
- Chapter 0952 and YY/T 1627-2018 both have peel strength and holding power tests, but they are different methods in different documents, and one result cannot stand in for the other.
The standard and its scope
The 2025 Edition of the Chinese Pharmacopoeia was issued by the National Medical Products Administration (NMPA) and the National Health Commission in Announcement No. 29 of 2025, dated 20 March 2025, and came into force on 1 October 2025. Attachment 4 to the announcement, the table of contents for the general requirements and guidelines (通用技术要求和指导原则目次), lists "0952 黏附力测定法" (adhesion test method) under the heading "0900 特性检查法" (property tests). The same list also includes the dosage-form chapters for patches (0121) and plasters (0122).
Chapter 0952 opens by stating that it measures how strongly plasters and patches adhere to the skin surface once applied. In the chapter's definitions, initial tack is the adhesion produced when the adhesive surface touches the skin under light pressure; holding power reflects the ability of the adhesive mass to resist deformation or failure under a sustained force; peel strength is the resistance of the adhesive mass to being peeled from the skin; and adhesive force is the adhesion the adhesive surface exerts on the skin after application.
The chapter was written for medicinal products. Device makers borrow it because cooling patches, acupoint pressure patches and adhesive dressings are mostly a backing plus an adhesive layer and need the same "goes on, stays on, comes off" measures. Remember that the chapter tells you how to test, not what limit a device must meet.
| Method | Indicator | Principle (summary) | Within SUNGO's accredited scope? |
|---|---|---|---|
| Method 1 | Initial tack | Rolling ball on an incline: a series of steel balls roll over the adhesive face of a specimen fixed to an inclined plate, and initial tack is rated by the largest ball number the specimen holds | Yes (Shanghai, CNAS and CMA) |
| Method 2 | Holding power | The specimen is applied to a vertical test plate with a specified weight hung along its length; the time to slip off, or the displacement over a set time, is recorded | No; commission separately |
| Method 3 | Peel strength | 180° peel: the adhesive face is bonded to polyester film, which is peeled continuously at constant speed on a tensile tester, and peel strength is calculated | Yes (Shanghai, CNAS and CMA) |
| Method 4 | Adhesive force | A dedicated adhesive force apparatus runs a roller over the adhesive face of a specimen held in a clamp, and a sensor measures the force | No; commission separately |
Method 1: initial tack
Apparatus
The set-up consists of an inclined plate, a base, stainless steel balls and a ball catcher. The inclined plate is stainless steel, set at 15°, 30° or 45° as the monograph specifies. Two horizontal lines are marked on it: the upper line is the ball's starting point and the lower line marks where the top of the specimen is fixed. The base keeps the apparatus level, the catcher is lined with soft material, and ball numbers and sizes follow the chapter's ball table.
Specimens and conditioning
Before testing, the specimens, still in their packaging, are held at 18–25 °C and 40%–70% relative humidity for at least 2 hours. The inclined plate and the balls are wiped with anhydrous ethanol and dried with a lint-free cloth, repeated at least three times until they look clean.
Procedure
Set the plate to the specified angle and take 3 specimens. Fix each by its backing to the plate with double-sided tape, with the top edge on the lower line, the adhesive face up and the test length along the slope no more than 5 cm, lying flat. Place the specified ball on the upper line, let it roll freely down the slope, and see whether the adhesive face holds it.
Judgement
Look at the ball each of the 3 specimens holds. If all 3 hold the largest ball number, or 2 hold the largest and the third holds a ball only one number smaller, the result conforms. If only 1 holds the largest and the other 2 hold balls one number smaller, a retest on 3 further specimens is required, and all 3 must hold the largest ball number to conform.
The incline angle and the "largest ball number" both come from the monograph. The same ball is harder to hold on a steeper plate, so a device's requirement should state angle and ball number together.
Method 3: 180° peel strength
Apparatus
A tensile tester, a stainless steel test plate, polyester film and a pressure roller. The chapter sets requirements for where the failure load sits within the tester's full scale, for force indication error, for constant-speed peeling and for automatic recording of the peel load, and specifies the plate and film. Conditioning is the same as for Method 1.
Procedure
- Fix the specimen's backing to the test plate with double-sided tape. If needed, tape down the upper and lower edges so the specimen lies flat.
- Bond the adhesive face to clean polyester film and roll it back and forth three times with a 2000 g roller so that no air bubbles remain.
- Leave the bonded specimen at room temperature for 20–40 minutes before testing.
- Fold the free end of the film back through 180°, clamp the film end and the test plate in the upper and lower grips, keep the peel plane in line with the tester's axis, and peel continuously at 300 mm/min ± 10 mm/min.
Note that in Method 3 the polyester film bonded to the adhesive face is what gets peeled, while the specimen is fixed to the steel plate. Common tape practice is the reverse (adhesive face on a steel plate, tape peeled off), so an in-house check using that set-up will not match.
Calculation and judgement
The 180° peel strength is calculated from the peel load over the evaluated section of the recorded curve and the actual specimen width, expressed in kN/m, and the result is the arithmetic mean. For pass or fail, the chapter only refers to the monograph, which for a device means the limit in its technical requirement. Agree in advance how the evaluated section of the curve is defined (for example, whether the start and end are discarded) so retests use the same basis.
How to cite Chapter 0952 in a device's product technical requirements
Chapter 0952 hands the Method 1 angle and ball, and the acceptance judgement for Methods 2 to 4, to the monograph. A device has none, so its technical requirements must supply them.
The NMPA guideline on writing medical device product technical requirements (医疗器械产品技术要求编写指导原则), issued by NMPA in 2022, makes three relevant points: performance indicators must state specific requirements, not "see attached documents" or "per the supply contract"; applicable established standard methods should be preferred, with method validation where necessary for reproducibility and workability; and cited national or industry standards must carry their number and year. For the Pharmacopoeia, give the edition year, chapter and method number in the same way.
In practice:
- Cite the basis in full, for example "ChP 2025 Edition, Volume IV, General Chapter 0952, Method 1" or "Method 3", not just "ChP 0952".
- For Method 1, state the incline angle (one of 15°, 30° or 45°) and the ball number that must be held.
- For Method 3, state the peel strength limit in the chapter's unit (kN/m). Whether to add an upper limit is for the manufacturer to decide, based on how removal feels on the skin and on the product design.
- If the shape or size makes standard specimens impractical (a round patch, or one with a raised part or gel pad in the middle), state where and how specimens are cut as an "unless otherwise specified" provision and consider method validation. Confirm before ordering whether the modified method still falls under the accredited "Chapter 0952, Methods 1 and 3".
- Holding power and adhesive force, if required, are outside SUNGO's scope and must be commissioned separately.
| Performance indicator (template) | Test method (template) |
|---|---|
| Initial tack: at an incline angle of ___°, the specimen shall hold ball No. ___. | Test according to ChP 2025 Edition, Volume IV, General Chapter 0952, Method 1. |
| Peel strength: 180° peel strength shall be not less than ___ kN/m. | Test according to ChP 2025 Edition, Volume IV, General Chapter 0952, Method 3; state any deviation explicitly. |
The blanks are for the manufacturer to set from its product design and verification data. SUNGO does not recommend limits.
Some cooling patch requirements in the NMPA filing database do not cite Chapter 0952 at all but define their own check, in which a single steel ball must stay on an inclined specimen for a set time. Such a self-defined method is not ChP 0952 Method 1 and cannot be reported under that accredited item; whether it can be taken on must be agreed before ordering.
How it differs from holding power and peel strength in YY/T 1627-2018
YY/T 1627-2018, General requirements of acute adhesive wound dressing and woundplast, is a recommended pharmaceutical industry standard published on 7 November 2018 and in effect since 1 November 2019. It applies to acute wound dressings and woundplasts made mainly of an adhesive layer, an absorbent pad and a release layer, but not to hydrocolloid products or products containing antimicrobial substances such as silver or chitosan. Its holding power (6.4.2, Annex B.1.2) and peel strength (6.4.3, Annex B.1.3) tests have their own test methods (refer to the standard for test conditions and acceptance); a separate article covers them in detail.
| Aspect | ChP General Chapter 0952 (Methods 1 and 3) | YY/T 1627-2018 |
|---|---|---|
| Type of document | General test method in ChP Volume IV, written for medicated plasters and patches | Recommended pharmaceutical industry standard for acute wound dressings and woundplasts |
| Adhesion indicators | Initial tack (Method 1), peel strength (Method 3); holding power is Method 2 | Holding power, peel strength |
| Acceptance | Left to the monograph; a device must state it in its technical requirements | Refer to the standard text for acceptance |
| SUNGO Shanghai accreditation | CNAS and CMA, test object "medical devices", Methods 1 and 3 only | CNAS and CMA, test object "adhesive dressings and woundplasts" |
Two points are easy to mix up:
- Holding power under Chapter 0952 (Method 2) and holding power under YY/T 1627 are different methods. SUNGO is accredited for the YY/T 1627 test (test object: adhesive dressings and woundplasts), not for Chapter 0952 Method 2.
- Both call their test "peel strength", but preparation, dwell and calculation follow each document's own rules, so a Chapter 0952 Method 3 report cannot be used against a YY/T 1627 clause, or vice versa.
Accredited scope
Relevant lines from the Shanghai laboratory's scope schedules:
| Item | Basis and clause | Notes and limitations |
|---|---|---|
| Adhesion | Pharmacopoeia of the People's Republic of China, 2025 Edition, Volume IV, General Chapter 0952 | CNAS L22083; test object "medical devices"; Methods 1 and 3 only |
| Adhesion | Pharmacopoeia of the People's Republic of China, 2025 Edition, General Chapter 0952 | CMA 240015340087; test object "medical devices"; Methods 1 and 3 only |
| Holding power | YY/T 1627-2018 6.4.2, Annex B.1.2 | CNAS L22083; test object "adhesive dressings and woundplasts" |
| Peel strength | YY/T 1627-2018 6.4.3, Annex B.1.3 | CNAS L22083; test object "adhesive dressings and woundplasts" |
| Holding power | YY/T 1627-2018 (no clause number in the schedule) | CMA 240015340087; test object "adhesive dressings and woundplasts" |
| Peel strength | YY/T 1627-2018 (no clause number in the schedule) | CMA 240015340087; test object "adhesive dressings and woundplasts" |
The only Pharmacopoeia item in the Shanghai IAS scope (TL-1019) is Section 1101 (sterility test), accredited for medical device testing only; Chapter 0952 and YY/T 1627 are not included. None of these lines is in the Hefei laboratory's scopes. To check accreditation marks and scopes on a report, see How to Check an Accreditation Scope and Read the Mark on a Report.
Where SUNGO performs it, and under which accreditation
- Laboratory: Shanghai SUNGO Medical Technology Co., Ltd., with its laboratory at Kangqiao East Road 958, Pudong, Shanghai. Hefei SUNGO Medical Technology Co., Ltd. is a separate legal entity whose scope does not include this item.
- Reports: Chapter 0952 Methods 1 and 3 can be reported with the CNAS or CMA mark. The CMA mark covers only items in the CMA schedule and, as the certificate states, is valid within the People's Republic of China. No IAS report can be issued for this item.
- Edition: the scopes list the 2025 Edition of the Pharmacopoeia. If your technical requirement still cites the 2020 Edition, confirm the basis with the laboratory before ordering.
- Biological tests: if the product also needs biological tests such as cytotoxicity, sensitisation or irritation, SUNGO subcontracts them to laboratories with the relevant qualifications. Under accreditation rules, the client's agreement is obtained before subcontracting, and the report identifies the subcontracted items and the subcontractor.
- Use outside China: Chapter 0952 is a Chinese Pharmacopoeia method. Whether a report can be used elsewhere is for the client to confirm with the relevant regulator or notified body; SUNGO makes no promise on acceptance.
Preparing samples
- Exact clause text: send the adhesion indicator and test method from your technical requirements (or draft), with edition, chapter, method number, incline angle, ball number and peel limit. Complete the clause before testing if anything is missing.
- Original packaging: the chapter conditions specimens together with their packaging. Keep the smallest sales unit sealed, and do not open it or remove the release liner in advance.
- Transport and storage: for gel-containing products such as cooling patches, avoid heat and freezing in transit. If there are specific storage conditions, state them on the test order.
- Sizes and specimen preparation: state the size submitted and, for irregular shapes, where and how specimens are cut. Method 3 uses the actual specimen width, so preparation affects the result.
- Quantity: Method 1 uses 3 specimens per judgement, plus another 3 if a retest is triggered. For Method 3, the number of specimens follows your technical requirement. Allow a margin for retesting and confirm the quantity with the laboratory.
- Product information: lot number, manufacturing date, and whether the product is sterile.
Frequently asked questions
Our technical requirement only says "adhesion per ChP 0952". Which method will the laboratory use?
The chapter number alone does not say which of the four methods applies and gives no acceptance basis. The client needs to confirm the method and parameters; we recommend amending the requirement to add them.
Can SUNGO test holding power (Method 2) or adhesive force (Method 4)?
No. These two methods are outside SUNGO's accredited scope and must be commissioned from a body with the relevant capability. SUNGO Shanghai is accredited for Method 1 (initial tack) and Method 3 (peel strength).
Can a Chapter 0952 Method 3 peel report be used as the YY/T 1627 peel strength result?
No. They are different methods in different documents. Test and judge to whichever document your technical requirement cites.
Can you issue an IAS report for an overseas customer?
No. SUNGO Shanghai's IAS scope does not include Chapter 0952. Whether an overseas customer or regulator accepts a CNAS report is for the client to confirm in advance.
Requesting a quote
For a quote, send the product name and construction (backing, adhesive and release liner materials), sizes, the exact adhesion clause from your technical requirements, the report type (CNAS or CMA) and any other tests needed. Other tests for dressing products such as acute wound dressings and woundplasts are listed under mask, glove, dressing and gauze testing services. To request a quote, use the contact page.
About SUNGO Lab: What We Test
SUNGO Lab is made up of two independent companies, Shanghai SUNGO Medical Technology Co., Ltd. and Hefei SUNGO Medical Technology Co., Ltd., and focuses on medical device testing. Our core service lines are:
- Wheelchair and mobility aid testing (Hefei laboratory): manual and powered wheelchairs, scooters, walking aids and crutches to the ISO 7176 series (excluding Part 19 crash testing and Part 20 standing wheelchairs), ANSI/RESNA WC-1/WC-2, EN 12183, EN 12184, the GB/T 18029 series and GB/T 12996-2024. Which accreditation (CNAS, CMA or IAS) covers each standard is as listed in our certificate scopes. See Wheelchair testing for FDA 510(k) and RESNA.
- Medical electrical safety and EMC (Hefei laboratory, IAS accredited, certificate TL-1119): IEC 60601-1, IEC 60601-1-2, IEC 60601-1-8, IEC 60601-1-11 and ISO 80601-2-69, with the corresponding Chinese standards GB 9706.1 and YY 9706.102.
- Testing for registration in China and overseas: we plan testing to the standards your target market requires (NMPA, FDA 510(k), EU CE marking and others) and issue the test reports for your submission; whether a report is accepted is decided by the regulator.
Our Shanghai laboratory also tests medical masks, gloves, surgical gowns, sterile packaging and sterilization-related items. CNAS and IAS are both signatories to the ILAC MRA. Send your product, target markets and standards through our contact page and we will confirm which laboratory and which accredited scope covers each test.